Axial-flux machines are usually presented as a packaging story: shorter, lighter, higher torque density than a radial machine of the same envelope. The packaging claim is true, and it is also the reason axial-flux programmes are harder to industrialise than they look.
In a radial machine the air gap is set by one machined diameter. In an axial machine it is set by a stack of parts along the shaft — rotor disc, magnets, bond line, stator, bearing play, thermal expansion — and every one of those tolerances lands directly in the gap. The magnet assembly is where most of that stack is created.
What makes axial-flux rotor magnet assembly different?
An axial flux rotor magnet assembly is a disc of thin sector magnets bonded to a rotor yoke, with the air gap set axially by a mechanical stack rather than by a bore diameter. Two consequences dominate: the gap is far more sensitive to thermal expansion and bearing play, and the magnets are thin enough (2–4 mm) that their permeance coefficient — and therefore their demagnetization margin — is low.
Key takeaways
- Topology decides the tolerance problem before any magnet is chosen. A yokeless dual-rotor machine removes iron from the axial stack and improves torque density, but it makes the gap dependent on the relative position of two discs, one of which is usually the one being cooled.
- The axial gap moves with temperature. Differential expansion between a steel rotor and an aluminium housing over a 100 °C rise reaches roughly 0.1 mm at a 100 mm radius — the same order as the gap itself. This must be designed, not measured after the fact.
- Thin magnets lose demagnetization margin in proportion to their thickness. Permeance coefficient scales roughly with magnet thickness over effective gap, so halving thickness roughly halves the margin at unchanged gap. A 2 mm design and a 4 mm design are not the same electromagnetic problem.
- Sector magnets are a lapping and parallelism problem, not a pressing problem. Arc segments in the 2–4 mm range distort during sintering, slicing and coating; flatness and thickness tolerance across the sector determine both the bond-line and the effective gap.
- The assembly force is the design constraint. Two rotor discs attract each other across the stator, and a thin magnet snaps onto a steel yoke with enough energy to crack itself. Fixtures and retention are designed around this force, not around handling convenience.
- Carbon-fibre wrapping and adhesive solve different problems. The wrap carries hoop and burst load; the adhesive carries shear and keeps the magnet located. A design that relies on adhesive for retention at high speed is relying on the wrong mechanism.
1. Topology first: what the rotor stack has to do
1.1 Yokeless dual-rotor (torque-dense, tolerance-hungry)
The dominant axial-flux traction topology is a single stator with a rotor disc on each side — a dual rotor axial flux topology with no stator yoke. Removing the yoke shortens the magnetic path and the axial length simultaneously, which is where the torque-density advantage comes from.

What it costs:
- Two air gaps instead of one, each set independently. Total axial error is the sum of both, and the two gaps interact magnetically: an asymmetry between them produces an unbalanced axial force that pushes the assembly further off centre.
- The stator is in the middle and usually the hottest part, so the gap on each side sees the differential expansion between a hot stator and two rotor discs whose temperatures may differ from each other.
- No yoke means no structural stiffness from the stator, so rotor disc stiffness and flatness become the machine’s dimensional backbone. A disc that deflects under magnet attraction changes the gap on both sides at once.
1.2 Single-rotor, double-stator and cored variants
The alternative family puts one rotor between two stators, or keeps a yoke in the stator. These trade axial length for:
- A single gap-setting surface per side, which is easier to control in production
- A stiffer stator structure, so the rotor disc can be thinner
- Better heat path from the stator to the housing, at the cost of axial length
The choice usually comes down to which tolerance the manufacturing base can actually hold. A topology that is 8 % better on paper but requires two independently controlled gaps within a few hundredths of a millimetre is a worse topology for a plant that cannot hold them.
1.3 Where hub motor magnet assembly fits
In-wheel and hub applications use the same axial-flux architecture with a different constraint set: the rotor diameter is set by the wheel, the axial length is heavily restricted, and the assembly must survive road-induced shock loads in addition to centrifugal load.
The magnet assembly consequence is that retention moves from “adequate” to “fail-safe”. A bonded magnet that releases in a hub motor becomes debris inside a rotating wheel. Designs in this category normally add mechanical capture — a wrapped band, a retaining ring, or a pocketed yoke — rather than relying on the bond alone.
1.4 Topology comparison
| Criterion | Yokeless dual rotor, single stator | Single rotor, double stator | Cored single-sided |
|---|---|---|---|
| Axial length | Shortest | Longer — two stator stacks | Longest — yoke plus stator |
| Torque density | Highest | High | Lowest of the three |
| Air gaps to control | Two, independent | Two, one per side | One |
| Gap sensitivity to thermal growth | Highest — three bodies at different temperatures | High | Lowest |
| Stator cooling | Good — both faces exposed to coolant or air | Good, but sandwiched rotor is hard to cool | Yoke conducts heat to housing |
| Rotor disc stiffness needed | High | Moderate | Low |
| Magnet assembly risk | Two live discs attracting each other | One live disc, two attraction paths | One disc, one attraction path |
| Typical production difficulty | Highest | Medium | Lowest |
Send your disc geometry for a gap-stack review →
2. Air-gap tolerance: the budget that decides whether the design works
An axial-flux machine’s nominal gap is often between 0.8 and 1.5 mm. Every term in the axial stack eats into it, and the terms are not small.
2.1 The tolerance stack
| Contribution | Typical magnitude | Notes |
|---|---|---|
| Rotor disc flatness and runout | 0.02–0.05 mm | Depends on disc thickness and machining |
| Magnet thickness variation | 0.02–0.05 mm | Across a sector, and sector to sector |
| Bond-line thickness variation | 0.02–0.10 mm | Controlled by dispensing and fixture pressure |
| Stator stack thickness | 0.03–0.10 mm | Stator stack or potted core |
| Bearing axial play and preload | 0.02–0.05 mm | Sets the dynamic variation |
| Thermal growth differential | up to 0.10 mm | See §2.2 |
| Assembly and clamping distortion | 0.02–0.05 mm | Often the least characterised |
Summed worst-case, these consume a substantial fraction of a 1 mm gap. The point is not the exact numbers — they vary by design — but that no single term dominates, which means no single supplier can be blamed. The gap is a system tolerance, and the magnet assembly contributes two of its terms.
Two practical consequences:
- The bond line is a controlled dimension, not an outcome. A dispense process that varies by 0.05 mm across a sector is 5 % of the gap, and it also tilts the magnet, which changes the effective gap further.
- Measure the gap on the assembled machine, not on the parts. Dimensional inspection of the magnet disc tells you the disc is good; it does not tell you the machine has a gap.
2.2 Thermal growth: a worked example
The differential expansion between a steel rotor and an aluminium housing is large enough to matter:
- Steel CTE ≈ 11–12 ppm/K; aluminium ≈ 23 ppm/K; difference ≈ 11–12 ppm/K
- At a 100 mm radius, with a 100 K temperature rise:
0.100 m × 100 K × 12×10⁻⁶ ≈ 0.12 mm
That is 0.12 mm of relative axial movement on a gap that may be 1 mm. It is not a second-order effect; it is the same order as the gap itself.
This is why axial-flux thermal design is inseparable from the magnet assembly: the material of the rotor yoke, the thickness of the bond line and the stiffness of the disc all feed into whether the gap closes, opens, or tilts as the machine heats. A design that closes the gap on one side and opens it on the other develops an unbalanced axial force, which loads the bearing and, in the worst case, produces a rub.
3. Thin sector magnet manufacturing: where 2 mm and 4 mm diverge
3.1 Why the magnets are thin, and what it costs
Axial length is the whole point of the topology, so magnets are specified as thin as the magnetic design allows — commonly 2 to 4 mm. Two penalties follow immediately.
Demagnetization margin falls with thickness. For a surface magnet on a yoke, the permeance coefficient scales roughly with magnet thickness over effective gap. Halving the thickness roughly halves the margin at unchanged gap, so a 2 mm design does not inherit the fault tolerance of the 4 mm design it replaced. Designs at the thin end therefore tend to require a higher coercivity grade for the same operating temperature — which is a cost that appears in the magnet, not in the assembly.
Manufacturing tolerance becomes a larger fraction of the part. A ±0.03 mm thickness tolerance is 1.5 % of a 2 mm magnet and 0.75 % of a 4 mm one, and the same absolute flatness error tilts a thin magnet further for a given bond-line pressure.
3.2 The tolerances that actually matter on a sector magnet
For segmented arc magnets for axial flux, five geometric characteristics matter, and they are not equally weighted:
| Characteristic | Why it matters |
|---|---|
| Thickness and parallelism across the sector | Sets the bond-line and the effective gap; a wedge-shaped sector tilts in the pocket |
| Flatness (both faces) | Determines whether the bond line is uniform and whether the magnet sits without rocking |
| Arc radius and sector angle | Sets the gap at the inner and outer radius; error produces a radial flux gradient |
| Width and gap between sectors | Sets the effective pole area and the harmonic content |
| Chamfer and edge quality | Thin parts chip at edges; chips become loose magnetic debris |
Note what is absent: absolute dimensional accuracy is less important than consistency across the set. A disc whose sectors are all 0.02 mm thin produces a uniform gap error, which the design can absorb. A disc whose sectors vary by 0.05 mm produces a once-per-revolution variation that shows up as vibration and as flux asymmetry.
This is also the argument for edge chamfer control: a 2 mm magnet with a chipped edge loses a visible fraction of its pole area, and the chip itself is a magnetic particle loose inside a machine.
3.3 What to require from a disc motor permanent magnet supplier
The specification that works is a set specification, not a part specification:
- Thickness distribution across the delivered set, not only per-part tolerance
- Parallelism and flatness stated with measurement method
- Coating thickness uniformity, since a 2 mm part with a 0.02 mm coating is 1 % coating — and coating variation adds directly to the gap tolerance
- Magnetization orientation stated as an axis relative to the part, with the allowed angular error
- Handling: sectors delivered in an ordered, non-magnetic tray keyed to position, not in bulk
- Flatness measured after coating, not before — coating and curing move thin parts
The last point catches more suppliers than any other. A supplier that inspects before coating is certifying a part that no longer exists.
3.4 Magnetization orientation consistency
In an axial-flux rotor, each sector’s easy axis must be normal to the disc face, and the polarity must alternate correctly around the ring. Two failure modes arise:
Ask for the per-sector orientation record →
- Angular error in the easy axis, which reduces the axial component and introduces an in-plane component that does nothing useful and adds to leakage.
- Sequence error — one sector magnetized with reversed polarity. Electrically this behaves like a missing pole: torque drops, flux asymmetry rises sharply, and the fault is often diagnosed as a stator problem before anyone checks polarity.
Polarity and orientation should therefore be verified per sector, not per batch, and the verification record should be tied to the disc’s serial number.
4. Retention under axial attraction
4.1 The attraction force is large and it is the fixture design driver
The axial pressure between a magnet face and a steel yoke in contact is approximately:
p = B² / (2·μ0)
For a working flux density of 0.6 T, p ≈ 0.36 / (2 × 1.2566×10⁻⁶) ≈ 143 kPa, or about 0.15 MPa. On a 20 cm² sector that is roughly 290 N — nearly 30 kg pulling a 2 mm thick part onto a steel disc, with no standoff and no damping.
Two things follow:
- Manual placement is not viable. The part accelerates over the last millimetre of travel, arrives with impact energy, and cracks or chips. Assembly fixtures use guided descent with a controlled air gap, often a non-magnetic shuttle that draws the magnet into place and is then withdrawn.
- Disc-to-disc attraction matters in dual-rotor builds. Two rotor discs, each carrying magnets over a steel yoke, attract each other across the stator. That force loads the bearings during assembly and, if the build fixture does not control it, closes both gaps simultaneously — which is exactly the condition the fixture exists to prevent.
4.2 Why hub motor magnet assembly needs fail-safe retention
In a hub or in-wheel machine, a released magnet is not a performance problem — it is a debris problem inside a rotating assembly, with brake and suspension components nearby.
Design practice in this category relies on mechanical capture as the primary retention: a pocketed yoke, a shoulder, a retaining ring, or a full wrap. The adhesive then performs its real job, which is to prevent micro-movement and fretting rather than to hold the part against centrifugal and shock loads.
4.3 Segmented arcs versus a continuous magnet ring
An axial flux motor magnet ring — a single continuous ring instead of discrete sectors — removes the inter-sector gaps and simplifies assembly to one bond operation. It also concentrates eddy-current loss, because a continuous ring provides a low-resistance path for circulating currents, and it makes repair impossible: one damaged zone condemns the ring.
Segmented arcs dominate in traction applications for three reasons: eddy loss is broken up by the gaps, individual sectors can be replaced or reworked, and the segmentation itself suppresses a class of circulating currents. The cost is part count and the tolerance stack of many bonds instead of one.
5. High-temperature bonding and what a wrap can and cannot do
5.1 Adhesive selection for a thin magnet on a steel disc
Three requirements drive the choice, and they pull in different directions:
Request an axial-flux bonding process review →
Shear strength at temperature. A structural toughened epoxy that performs well at 23 °C loses a significant share of its shear strength at 150–180 °C. Because the magnet is bonded to a yoke that also carries stator heat, the bond-line temperature is usually higher than the coolant temperature. Specify the strength at the service temperature, not at ambient.
Toughness rather than peak strength. Thin magnets on steel, cycled thermally, load the bond line in peel at the edges as much as in shear across the face. A brittle high-strength adhesive fails at the edge first; a toughened adhesive with lower nominal strength usually outlasts it.
Creep resistance. At elevated temperature, a thermoset under sustained load creeps. The sustained load here is the magnet’s own attraction to the yoke, which is permanent. A bond line that creeps releases preload and allows fretting, and fretting under a magnet is how coating damage starts.
Practical process requirements that determine whether any of this holds:
- Bond-line thickness controlled to a stated range, typically 0.1–0.25 mm, held by fixture rather than by operator pressure
- Surface preparation matched to the coating — an epoxy-coated magnet and a NiCuNi-coated magnet need different treatments, and a generic “clean and bond” instruction is where adhesion failures begin
- Cure profile qualified on the actual stack, since the steel yoke’s thermal mass dominates the ramp
- Void and coverage acceptance criteria with a defined inspection method, usually ultrasonic or visual on a witness coupon
5.2 What a carbon-fibre wrap actually resists
Carbon-fibre wrapping is standard on high-speed axial-flux rotors, and it is routinely misunderstood in one specific way.

A hoop wrap resists radial and hoop loads — the burst tendency of the magnet set and the disc’s own centrifugal growth. It does not resist axial peel, because the fibres run circumferentially and carry no axial load. A design that relies on a wrap to keep magnets from lifting off the disc has no axial retention at all beyond the adhesive.
That distinction matters in dual-rotor machines, where the axial attraction between discs is a sustained load in the direction the wrap cannot help with. Axial retention has to come from geometry — a pocket, a shoulder, a retaining ring, or a stepped bond surface.
Two further points on wraps:
- Pre-tension and CTE interact. Carbon fibre has a near-zero or slightly negative axial CTE while steel is around 11 ppm/K, so the wrap’s interference changes with temperature. Whether it tightens or loosens at operating temperature is a design calculation, not an assumption.
- The wrap changes the magnetic gap only if it sits in the gap. A wrap on the outer diameter or over the disc face adds axial thickness where it crosses the face, which must be included in the stack.
5.3 Thermal cycling is the real qualification
A single hot soak proves very little. The failure mode in bonded thin magnets is progressive: differential expansion between magnet, adhesive and steel loads the bond-line edges, micro-cracks initiate, and the joint loses area over cycles rather than all at once.
The qualification that catches this is thermal cycling between the cold and hot extremes, with the assembly under representative axial load, followed by shear testing of witness coupons and inspection for edge debonding. A programme that qualifies on a single elevated-temperature shear test has qualified the adhesive, not the assembly.
6. Specifying an axial-flux magnet assembly
| Item | What to state | Why it decides the answer |
|---|---|---|
| Topology | Yokeless dual rotor, single rotor double stator, or cored | Sets the number of gaps and the tolerance stack |
| Nominal air gap and allowed variation | Both gaps, with the variation budget | The single most important number in the design |
| Disc geometry | Outer and inner radius, disc thickness, material, flatness | Sets stiffness, flatness and thermal growth |
| Sector count and dimensions | Number per disc, arc angle, width, gap | Determines harmonic content and assembly sequence |
| Magnet thickness and grade | Thickness, grade, coating, temperature class | Thickness drives both demag margin and gap tolerance |
| Thickness distribution requirement | Variation across the delivered set, not only per part | Consistency governs the machine, not absolute accuracy |
| Parallelism and flatness | Values with measurement method, measured after coating | Determines bond-line uniformity |
| Bond specification | Adhesive class, bond-line range, cure profile, void limits | Sets retention and fatigue life |
| Axial retention | Pocket, shoulder, ring, or wrap — and which of these carries the axial load | A hoop wrap cannot provide axial retention |
| Hoop retention | Wrap specification, pre-tension, and CTE interaction | Burst margin at maximum speed |
| Bond-line service temperature | Maximum sustained and peak, not coolant temperature | Adhesive strength and creep are temperature-dependent |
| Verification | Per-sector polarity and orientation, disc-level flux map, bond-line inspection | Without these, the assembly cannot be confirmed as built |
The row that generates the most rework in practice is thickness distribution across the set. Buyers specify a per-part tolerance, receive parts that all comply, and then discover that the variation across the disc produces a once-per-revolution flux ripple. Specifying the set distribution costs a conversation with the supplier and prevents a redesign.
Frequently asked questions
What is an axial flux rotor magnet assembly? A disc of thin sector magnets bonded to a rotor yoke, with the air gap set axially by a mechanical stack rather than by a bore diameter. Both defining difficulties follow from that: the gap is sensitive to thermal expansion and bearing play, and the magnets are thin enough that their demagnetization margin is low.
Is a yokeless dual rotor better than a single rotor double stator? On torque density and axial length, usually yes, because removing the stator yoke shortens the magnetic path. It is also harder to build: two independent gaps must be controlled, and the two rotor discs attract each other across the stator. The better topology is the one whose tolerance stack the manufacturing base can actually hold.
Why is air-gap tolerance more critical in axial flux machines? Because the gap is the sum of a mechanical stack along the shaft rather than a single machined diameter. Rotor flatness, magnet thickness, bond line, stator thickness, bearing play and thermal growth all add directly to it, and differential expansion between a steel rotor and an aluminium housing reaches about 0.12 mm over a 100 K rise at 100 mm radius — comparable to the gap itself.
How thin can axial flux sector magnets be made? Two to four millimetres is the common production band. Below that, two things degrade together: the permeance coefficient falls with thickness, so demagnetization margin drops roughly in proportion, and manufacturing tolerance becomes a larger fraction of the part. A 2 mm design typically needs a higher coercivity grade than the 4 mm design it replaces.
Should an axial flux rotor use segmented arcs or one continuous ring? Segmented arcs dominate in traction applications: the gaps break up eddy-current paths, sectors can be replaced individually, and segmentation suppresses a class of circulating currents. A continuous ring simplifies assembly to one bond operation but concentrates eddy loss and cannot be repaired locally.
How are magnets retained at high speed in a hub motor? By mechanical capture rather than by adhesive alone. Pocketed yokes, shoulders, retaining rings and full wraps are standard, because a released magnet in a wheel is a debris hazard rather than a performance issue. The adhesive’s job is to prevent micro-movement and fretting.
Does a carbon-fibre wrap hold the magnets onto the disc? Only in the radial and hoop direction. A circumferential wrap carries no axial load, so it cannot prevent magnets from lifting off the disc face. Axial retention must come from geometry — a pocket, a shoulder or a retaining ring — particularly in dual-rotor machines where the discs attract each other.
What temperature must the bond line survive? The sustained temperature at the bond line, which is typically higher than coolant temperature because the yoke carries stator heat, plus the peak from any hot-soak condition. Specify the adhesive’s shear strength and creep resistance at that temperature, not at ambient, and qualify by thermal cycling rather than by a single hot soak.

AXIAL-FLUX MAGNET ASSEMBLY
Building a disc rotor and not sure the gap stack will hold?
Disc diameter, the axial stack, the magnet thickness and the worst-case temperature are enough for our engineers to run the tolerance budget, the attraction force on the assembly fixture and the retention requirement. If it is axial flux, the enquiry is already classified as one.
- Reviewed by electromagnetic engineers, not a sales desk
- Typical reply within one business day
- Disc geometry and axial stack are enough to start
Prefer to talk it through? WhatsApp +86 188 6892 9496
Published 18 November 2026 · Reviewed by the JHHS MAG magnetizing engineering team
JHHS MAG (Ningbo Jiuheng Huisheng Technology Co., Ltd.) designs capacitor-discharge impulse magnetizers, magnetizing coils and fixtures, and automated magnetizing and testing systems for motor and magnetic component production. This article is part of the magnetizing knowledge base.
Continue reading
- Halbach array rotor design — what a segmented or Halbach arrangement changes on a magnet disc
- Multi-axis flux mapping for traction rotors — how the finished disc is verified, sector by sector
- High-temperature NdFeB for EV traction motors — why a 2 mm magnet needs a higher coercivity grade